Researchers have broken the 25 percent efficiency barrier for n–i–p all-perovskite tandem solar cells, reporting a certified 25.3 percent conversion rate for a small-area device and 24.7 percent for a 1.045 cm² cell, Nature reported on Friday.
- First n–i–p all-perovskite tandem to exceed 25 percent efficiency, reaching 25.3 percent on a 0.096 cm² cell and 24.7 percent on a 1.045 cm² cell.
- Interconnection layer engineering — MeO-2PACz on P3HT and PCBM on ALD-SnO₂ — solves the thermal budget mismatch that has long confined high-efficiency tandems to p–i–n architectures.
- Stacking the n–i–p double junction with a 1.25 eV p–i–n subcell in a four-terminal triple-junction configuration pushes efficiency to 28 percent.
The breakthrough centers on a 2.0 eV cesium-based all-inorganic wide-bandgap top subcell paired with an additive-free P3HT hole-selective contact. Historically, n–i–p integration has lagged because the preformed top cell and its hole contact must survive the thermal processing of the bottom subcell, a constraint that limited material choices and capped performance.
By reconfiguring the molecular organization of P3HT with MeO-2PACz, the team enhanced hole extraction and eliminated a transport bottleneck at the interconnection layer. Simultaneously, modifying the ALD-SnO₂ electron-selective contact in the 1.55 eV bottom subcell with PCBM balanced carrier coupling, suppressed charge accumulation, and cut voltage losses.
Stabilized power output for the 1.045 cm² device held at 24.4 percent, confirming operational stability near the peak efficiency. The architecture also enables a four-terminal triple-junction device: coupling the n–i–p double junction with a narrow-bandgap 1.25 eV p–i–n subcell delivered 28 percent efficiency, the highest reported for an n–i–p-based triple junction.
Monolithic tandems require the top subcell to withstand bottom-cell fabrication temperatures. In p–i–n stacks, the top cell is deposited last, avoiding thermal stress. In n–i–p stacks, the wide-bandgap top cell — typically organic–inorganic — degrades during bottom-cell processing.
The 2.0 eV Cs-based all-inorganic top cell solves the thermal stability problem, but its hole contact remained a weak link until the MeO-2PACz treatment ordered the P3HT chains for efficient extraction.
The n–i–p route offers potential manufacturing advantages: the electron-selective SnO₂ layer is deposited by atomic layer deposition (ALD), a technique already standard in display and semiconductor fabs, and the P3HT hole contact is solution-processed without additives.
Durability under continuous illumination, thermal cycling, and humidity remains the critical unproven metric. The paper reports stabilized output at maximum power point but does not publish IEC 61215 damp-heat or light-soaking data. Scaling the ALD SnO₂ process to module widths while maintaining uniformity and throughput will determine whether the efficiency gains translate to production lines.
Nature reported the results as the first n–i–p double-junction device exceeding 25 percent and the first n–i–p-based four-terminal triple junction reaching 28 percent.